Instructions and precautions
1.more than the machine for 157g paper thickness of less than 157g of paper,please test to use.In the event of the phenomenon of sticky film eject in time,less than 157g of paper must be thick tail,and pull the paper out of paper at the manual.Laminating phase to be sure to roll up the image side out.
2.To ensure that the paper surface before lamination dry cleaning,no impurities,the front-end formation.Automatically be closed after the observation of the paper is normal into the uv curing machine ((not waterproof paper and laser film lamination is the best 5.5-7 m / min,about 30-60 in the values between.RC waterproof paper and paper speed of less than 200g slowly to avoid sticky roller,specific test to confirm.) long piece of cardboard at the need to take tablets,so that the whole film full uniform through the UV curing machine.the film surface after the hand-lamination and stick with a soft towel to wipe the water repeatedly confirm the curing is complete,observe the laminated surface is uniform.
3.Some RC waterproof photo paper + pigment ink Laminating be twice
4.4 IR function is to assist the leveling effect can be more bright and smooth.
5.Infrared leveling opened two minutes later to work properly,open the lamination is the plane of polarization effects,the IR infrared control knob to regulate the temperature.Too bad baking paper and may affect the curing,low surface lamination smoothness and brightness will be somewhat less.adjusted to the specific test the best.
7.After the first working day can start by using the method used,usually do not clean the machine.As the Ministry of stainless steel feed roller glue lamination fluid.Just the machine for 1 minute,the scraper can be laminated liquid shave,after prolonged use can not be normal if there scraper shave lamination fluid situation,rotating blade to the visible position and clean with alcohol.And then wipe clean.Squeegee pressure adjustment screw can not be another overtighten.If still can not shave the blade may be the purpose of fine sandpaper abrasion graze 1500 required repair or replace blade.Blade life is generally 2-6 months.